EN AW-2007 22 x 3000 mm
EN AW-2007
An aluminium and copper alloy that typically contains between 4.0 and 5.0 % copper, and it is suitable for producing machine parts, bolts and rivets. It looks very much like EN AW-2011, but it is yet a bit harder. It is a short-chipped alloy, which is suitable for treatment, threads and high machining speeds. The alloy has a low corrosion resistance and is not suitable for welding because of the high content of copper. It is not approved by the ROHS.
We are not liable for items out of stock. The specified weight is theoretical. Please contact us if you have any further enquiries.
Alloys
Density | Si | Fe | Cu | Mn | Mg | Cr | Ni | Zn | Ti | Bi | Pb | Sn | Other | ||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Name | g/cm3 | Max | Max | Min | Max | Min | Max | Min | Max | Max | Max | Max | Max | Max | Min | Max | Max | Max | Rest |
EN AW-2007 | 2.85 | 0.8 | 0.8 | 3.3 | 4.6 | 0.5 | 1 | 0.4 | 1.8 | 0.1 | 0.2 | 0.8 | 0.2 | 0.2 | 0.8 | 1.5 | 0.2 | 0.3 | Al, Aluminium |
Aluminium Properties
Thermal conductivity | Coefficient of thermal expansion | Melting point | Elastic modulus | Electrical conductivity | |||
---|---|---|---|---|---|---|---|
Alloy | Temper | W/m*K | µm/(m*K) | min °C | KN/mm2 | %IACS | |
EN AW-2007 | T3 | 130 | 23 | 510 | 640 | 72 | 34 |
EN AW-2007 | T4 | 130 | 23 | 510 | 640 | 72 | 34 |
Mechanical properties
Dimension | Tensile strength (Rm) MPa | Proof stress (Rp0,2) | Elongation | Brinell Hardness | Elongation A50mm | ||||
---|---|---|---|---|---|---|---|---|---|
Norm | Alloy | Temper | Min | Max | Rm N/mm2 | MPa | % min | HBS | % min |
EN 755-2:2013 | EN AW-2007 | T4 | - | 80 | 370 | 250 | 8 | 95 | 6 |
EN 755-2:2013 | EN AW-2007 | T4 | 80 | 200 | 340 | 220 | 8 | 95 | - |
EN 755-2:2013 | EN AW-2007 | T4 | 200 | 250 | 330 | 210 | 7 | 95 | - |